Abstract

We have developed a vacuum mechanofusion system which maintains a residual pressure in the reaction chamber lower than 10-2 Pa during mechanofusion processing. Using this system, we success-fully coated Cu powders of 30μ m diameter with Al2O3 powders of 0.5μ m diameter.The effects of the residual pressure and the Al2O3 content on the mechanofusion behavior of Cu/Al2O3 particles were investigated by observing the particle size distribution and the appearance of the mechanofused particles. The mechanofusion behavior of Cu/Al2O3 particles strongly depended on the residual pressure, i.e., the volume percent of uncomposite particles decreased as the residual pressure became lower. The degree of coating promotion was dependent on the Al2O3 content. The adhesion of composite particles became stronger with decrease of Al2O3 content, especially when Al2O3 content was smaller than 1.0 wt%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.