Abstract

Abstract Nano-sized cobalt powder was fabricated by wet chemical reduction method at room temperature. Theeffects of various experimental variables on the overall properties of fabricated nano-sized cobalt powders have beeninvestigated in detail, and amount of NaOH and reducing agent and dropping speed of reducing agent have been prop-erly selected as experimental variables in the present research. Minitab program which could find optimized conditionswas adopted as a statistic analysis. 3D Scatter-Plot and DOE (Design of Experiments) conditions for synthesis of nano-sized cobalt powder were well developed using Box-Behnken DOE method. Based on the results of the DOE process,reproducibility test were performed for nano-sized cobalt powder. Spherical nano-sized cobalt powders with an averagesize of 70-100 nm were successfully developed and crystalline peaks for the HCP and FCC structure were observedwithout second phase such as Co(OH) 2 .Keywords: Nano-sized cobalt powder, Wet chemical reduction, Design of experiments, Reproducibility

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.