Abstract

The galvanostatic anodizing results of specially prepared high-purity aluminum in aqueous solutions of complex compounds K3[Co(C2O4)3] and K2[Zn(edta)] of various concentrations in the current density ranges 1.5–1.10·102 and 1.5−30 mA·сm−2, respectively. The kinetic features of anodizing have been established, indicating the occurrence of an oscillatory electrochemical process. Morphological features of a flaky and loose nature for K2[Zn(edta)] and monolithic for K3[Co(C2O4)3], uncharacteristic for anodic aluminum oxide, were revealed. The elemental composition, IR spectroscopic and photoluminescent characteristics of the formed oxides are shown.