Fracture toughness of WC-(4-20)%Ni alloys and WC-10%Ni alloys with different WC grain size (1.31-2.21μm) was compared with that of WC-Co alloy. Effect of various additions on the fracture toughness of WC-10%Ni alloy was also investigated.The results obtained are as follows:(1) Fracture toughness of WC-Ni alloy increases with the increase of the Ni content and the WC grain size.(2) WC-Ni alloy shows a fracture toughness equal to WC-Co alloy in relation to hardness. However, for the same WC grain size, the WC-Ni alloy shows a lower hardness and a higher fracture toughness than those of WC-Co alloy. The reason is considered to be in that the binder phase of WC-Ni alloy has lower hardness and higher fracture toughness.(3) By addition of Si, Ti, Cr and Mo which are soluble in Ni, the hardness of the WC-Ni alloy is increased. It is found that WC-Ni alloys containing 6%Si, 1-2%Ti, 5-10%Cr and Mo in the Ni binder show the same hardness and fracture toughness as the WC-Co alloy has.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.