Abstract

Recently the needs of ultra low [S] and ultra low [O] steel for many kinds of products increase.Secondary refining process to achieve less than 5 ppm sulfur and less than 10 ppm oxygen in molten steel was investigated. In order to produce ultra low sulfur steel the optimum slag composition was determined as 60%CaO-32%Al2O3-8%SiO2 and the deviation of final slag composition could be decreased by the method of 2 times flux addition.In the case of producing ultra low oxygen steel, it was important for increasing deoxidation rate that the total content of FeO+MnO in slag before RH process was less than 1 wt% and then deoxidizing products were removed through RH process. On the basis of these results, the refining process, BOF-VSC-NKAP-GI-RH process, was established. By this process it became possible to achieve less than 5 ppm sulfur and less than 10 ppm oxygen in steel.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.