The cellulose nanofibers (CNFs) were prepared by wet disk-milling (WDM) and fractionated by settling method into supernatant, middle and sediment fractions. The diameter and its distribution of the fractionated CNFs were investigated. With increasing WDM passing number, precipitation became delayed. Weight fraction at sediment fraction was decreased, whereas those at supernatant and middle fractions were increased with increasing WDM passing number. Diameter distribution of CNFs at supernatant fraction was narrowest and became broaden at middle and sedi- ment fraction. Filtration time was longer in order of supernatant, middle and sediment fraction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.