Abstract
Lithium manganese spinel (LiMn2O4) for Li-secondary battery was prepared by mechanical milling of raw materials in a argon atmosphere for 200 h. After milling and heating at 823 K for 3 h, the powder was observed X-ray diffraction pattern of lithium manganese spinel structure. The average milling powder diameter was approximately .0.1μm.The compounds of the MA-Li1.02Mn2O4 powder heated at 973 K for 3 h was evaluated as a 4 V cathode in a lithium non aqueous cell. The MA-Li1.02Mn2O4 have 136 Ah/kg of second discharge capacity.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Society of Powder and Powder Metallurgy
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.