Abstract

Cotton fibers were pretreated with aqueous sodium hydroxide solution (NaOHaq.), liquid ammonia (L.NH3) and their combination (NaOHaq/L. NH3). The effects of the pretreatments on Wash & Wear and mechanical properties of cotton fabrics finished with dimethyloldihydroxyethyleneurea (DMDHEU) and vapor-phase-formaldehyde (HCHO) were compared.The pretreatment effects on Wash & Wear properties and tensile strength of cotton fabrics crosslinked with DMDHEU and vapor-phase-HCHO were found to increase in the following order : DMDHEU : control<<NaOHaq.<NaOHaq/L. NH3_??_ L. NH3.HCHO : control_??_NaOHaq.<<NaOHaq/L. NH3 L.<NH3.It is likely that the results obtained in this experiment coincide with the size and distribution of porestructures of the pretreated fibers.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.