Abstract

It is necessary to reduce the debinding time in powder injection molding process. Therefore, recently, there are methods such as ANAX process of removing the binders and the solvent debinding which can solve the problems mentioned above becomes to get much attention. Here discussed solvent debinding of injection molded Fe-36%Ni with use of polyvinylbuthyral as organic binder. The all organic binders of the componud dissolved into the solvent in this process, although the all ones of the compound could not be always dissolved into the solvent on conventional solvent de-binding process. In this process, the sintered bodys scarely containing carbon were produced under these conditions ;(1) extraction binder volume was at least 30vol% after the solvent debinding process, and (2) after solvent debinding process, the optimum maximun temperature on thermal debinding process was 350°C in air.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.