Abstract

Nanoparticles of the alloy with the composition Nd-Fe-B were formed by the chemical method of co-precipitation reduction using a reducing agent sodium borohydride. The nanoparticle size was 35–95 nm. The silica coating was applied after stabilizing the nanoparticles with APTMS. The core of Nd-Fe-B alloy nanoparticles covered with a SiO2 shell, Nd2Fe14BаSiO2, the particle size was 35–125 nm with a shell width of 8–15 nm.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.