Aluminum hydroxides were synthesized by a simple electrolytic reaction of aluminum plates. The aluminum hydroxide, boehmite (AlO(OH)), was predominantly formed in the application of electrical potential at and above 30V, while the mixture of bayerite (<TEX>$Al(OH)_3$</TEX>) and boehmite (AlO(OH)) phases were formed below 20V. The boehmite has a clear fibrous structure controlled on nanometer scale. On the contrary, the bayerite consists of the typical hourglass or semi-hourglass shaped coarse crystals as a result of aggregation of various crystals stacked together. The specific surface area of the boehmite nanofiber was markedly high, approaching at about <TEX>$302\;m^2/g$</TEX>.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.