Modification of the composition and structure of heavy concrete with the use of a complex chemical-mineral additive consisting of fly ash from thermal power plants, a superplasticizer, a high-valence hardening accelerator AC and a fine-dispersed clinker component is considered. Modified concrete is characterized by an increase in compressive strength at a brand age by 67%, a decrease in the water content of a concrete mixture by 13.6% and an improvement in its workability by 11-12 cm. With the combined use of a superplasticizer and a high-valence hardening accelerator AC a significant synergistic effect is observed in the format of enhancing their plasticizing effect. The high efficiency of the application of the mixed-dispersed clinker component has been established.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.