We found that the optimal Si content of thermally stable Si-DLC film made by plasma based ion implantation technique with positive-negative high voltage pulses was about 21 at%. The technique can heat up specimens by electron bombardment with controlling the positive pulse voltage. In order to find the optimal positive pulse voltage in the process, we have examined the effects of the pulse voltage on several mechanical properties, such as internal stress, hardness, friction coefficient and wear resistance with controlling the positive pulse voltage as 2, 4 and 6.3 kV. The temperature increased, and internal stress and hardness decreased, with increasing the pulse voltage. The Si-DLC film with 4 kV pulses (about 570 K) is the largest thickness, the lowest friction coefficient and the highest wear resistance. The film has kept very low friction coefficient even after the annealing of 870 K, 3.6 ks in the Air.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.