Abstract

Rapidly solidified ribbons of 50 μm and 100 μm in thickness were prepared by a single roll method. Al6Fe, Al12Mo and Al3Fe precipitates are observed in quenched specimens of 100 μm thick ribbons but hardly observed in those of 50 μm thick ribbons. Using the 50 μm and 100 μm thick ribbons, two kinds of alloy bar were produced by hot extrusion at 723 K. The alloy bar made from 100 μm ribbons shows a higher 1000 h creep rupture strength at 573 K∼673 K than the bar made from 50 μm ribbons. The “n” value calculated from the equation e=k·σn is 7 and 9 for the bars made from 50 μm and 100 μm ribbons, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.