Abstract
The chemical compositions and properties of glass of different systems for the production of glass ionomer dental cements (GIC) were analyzed. For the synthesis of glass, the basic system 4SiO2–3Al2O3 – xNb2O5 – CaO with the content of Nb2O5 8.8 and 16.2% (wt.) is proposed. High-temperature technology and parameters of glass production for GIC are presented in the article. The
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Chemistry, Technology and Application of Substances
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.