Abstract

The possibility of using the "Brazilian test" method to determination the tensile strength σt of composite zirconia ceramics small-size samples were demonstrated and the reliability of the obtained σt values were confirmed. It was found that the dependence of the tensile strength of alumina toughened zirconia (stabilized by calcium oxide) with silica addition (CaO-ATZ+SiO2 ceramics) on SiO2 concentration in them has a maximum (σt = 450 MPa, at SiO2 = 5 mol.%). The observed toughened is explained by an increase in the transformability of the tetragonal t-ZrO2 phase and, accordingly, by an enhanced role of transformation toughening when SiO2 is adding into the ATZ ceramics.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.