Abstract

Опыт применения ингибитора солеотложений «НАЛКО 1392» в циркуляционной системе водоснабжения Нововоронежской атомной электростанции

Highlights

  • The water chemistry should ensure the operation of equipment without any damage to its components or the loss of efficiency caused by the corrosion of the internal surfaces as well as without scale and sludge formation

  • In the process of operating the circulating water supply system at the Novovoronezh nuclear power plant (NVNPP), heating leads to the cooling water oversaturation with salts, primarily, with calcium carbonate, this causing the formation of scale on the heat-exchange surfaces (Vlasova 2007, Vitkovskiy et al 2017)

  • An alternative way to cope with the negative effects of the high carbonate hardness of water is to maintain such water chemistry in the system with which the scale crystals formed are stabilized within the water column by the action of the salt scaling inhibitor and do not settle on the heat-transfer surface (Ivanova and Cherkasova 2016, Procedural recommendations)

Read more

Summary

Research Article

Experience of using the NALCO 1392 scale inhibitor in the circulating water supply system of the Novovoronezh NPP*. Academic editor: Elena Artyushkova ♦ Received 16 October 2020 ♦ Accepted 3 March 2021 ♦ Published 21 June 2021 Nuclear Energy and Technology 7(2): 85–89. https://doi.org/10.3897/ nucet.7.68940

Introduction
Liquid Transparent
Conclusions
Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call