Abstract

The effect of Li-addition to the low-Tc phase in Bi-Sr-Ca-Cu-O system have been studied for the samples with nominal compositions of Bi:Sr:Ca:Cu:Li=2:1.5:1.5:2-x:x heated at 720 to 845°C for 12 to 24h in air (x=0 to 0.8). The Li-addition promotes the formation of the low-Tc phase. Single phase of the low-Tc phase was obtained for the sample with x=0.2 to 0.4 more easily than the sample with x=0. The lattice constant c of the low-Tc phase increases as the Li content increases. As the heating period becomes longer, the amount of Li content in the low-Tc phase decreases.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.