Abstract
The synthesis of lithium conducting solid electrolyte Li1.5Al0.5Ge1.5(PO4)3 (LAGP) by liquid-phase method from oxalate and citrate precursors is investigated. The samples were characterized by XRD, DSC / TG, IR, impedance spectroscopy and potentiostatic chronoamperometry. It was found that the formation of a single - phase LAGP from an oxalate precursor occurs at a lower temperature (600–650 °C) and is preferable compared to the synthesis of LAGP from a citrate precursor. The ionic conductivity of the electrolyte was 4,2 · 10-4 S / cm, the electronic conductivity did not exceed 2 · 10-10 S / cm, the decomposition potential was 3.8 V.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of the Kоla Science Centre of RAS. Series: Engineering Sciences
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.