Abstract
We deposited <TEX>$Al_2O_3$</TEX> thin films on GaN by remote plasma atomic layer deposition (RPALD) technique, trimethylaluminum(TMA) and oxygen were used as precursors, at fixed process condition, the number of cycle were changed. Growth rate per cycle was <TEX>$1.2\;{\AA}$</TEX>/cycle. and Growth rate was in proportion to a number of cycle, the GaN MIS capacitors that <TEX>$Al_2O_3$</TEX> thin film were deposited above 12 nm, have excellent electrical properties, a low electrical leakage current density(<TEX>${\sim}10^{-10}\;A/cm^2$</TEX> at 1.5 MV), but below 12 nm, we can see the degradation of the leakage current density. After post deposition annealing, Dielectric constant was estimated by 1 MHz high-frequency C-V method, it was varied with the anealing temperature from 6.9 at no post anealed to 7.6 at <TEX>$800^{\circ}C$</TEX>, and we can see a improvement of the leakage current density and breakdown voltage by post deposition anealing below <TEX>$700^{\circ}C$</TEX>, but, after anealed at <TEX>$800^{\circ}C$</TEX>, we can see the degradation of the leakage current density and breakdown voltage.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Korean Institute of Electrical and Electronic Material Engineers
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.