Abstract

In this study the (Alnico, Sm-Co) bonded magnets were fabricated by mixing the Sm-Co added alnico alloy powders with epoxy resin and binder, appropriately. Also, the hybrid ring magnets of (Alnico, Sm-Co)/Sr-ferrite were fabricated by coupling the Sr-ferrite composite layer with an (Alnico, Sm-Co) magnet. The magnetic properties of (Alnico, Sm-Co) ring magnets were varied with the amount of Sm-Co powders. The addition of Sm-Co powders increased a remanent induction() and coercive force(), while decreasing a surface flux density and repulsive distance. The surface flux density and repulsive distance for the (Alnico, Sm-Co) ring magnet increased with a magnetizing voltage up to about 160 V and reached an apparent saturation point. Also, the measurements of temperature and moisture characteristics showed that the surface flux densities of N-S poles and repulsive distance decreased a little within 4% after 10 days passed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call