Abstract
In this research TiAl6V4 titanium base alloy was used for Selective Laser Melting (SLM). This alloy is widely used in aerospace and medical industries. For determination of influence of SLM process parameters on TiAl6V4 10x10x5 mm specimens were fabricated by using different SLM process parameters. The porosity of fabricated specimens was determined by microscopy analysis of cross-sections. The lowest porosity that was achieved is about of 0.5%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Russian Internet Journal of Industrial Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.