Abstract

This article represents a logical continuation of the research results presented in the previous publication and reflects the results of studies of the effect of the binder composition No. 3 (BC-3) on the formation of the microstructure and physical and mechanical properties of granular aggregates. The experimental results demonstrate that the best indicators of the strength of granular aggregates are provided with the adding of BC-3 in an amount of 15%, regardless of the fractional composition of quartz sand. In addition, the density of crystalline formations reflecting the microstructure of the samples directly affects the physical and mechanical properties of the composites. On dispersed micro fillers, as on a base plate, a dense microcrystalline structure of new formations of hydrated calcium silicates is formed. The addition of 15% binder composition No. 3 (BC-3) to the component composition of granular aggregates ensures the stability of physical and mechanical properties. Thus, they can be recommended for use as coarse aggregates in the preparation of special-purpose mortar mixtures

Highlights

  • ОСОБЕННОСТИ ФОРМИРОВАНИЯ МИКРОСТРУКТУРЫ ГРАНУЛИРОВАННЫХ ЗАПОЛНИТЕЛЕЙ НА РАЗНЫХ ВЯЖУЩИХ КОМПОЗИЦИЯХ (ЧАСТЬ 3)

  • This article represents a logical continuation of the research results presented in the previous publication and reflects the results of studies of the effect of the binder composition No 3 (BC-3) on the formation of the microstructure and physical and mechanical properties of granular aggregates

  • The experimental results demonstrate that the best indicators of the strength of granular aggregates are provided with the adding of binder composition No. 3 (BC-3) in an amount of 15 %, regardless of the fractional composition of quartz sand

Read more

Summary

Introduction

ОСОБЕННОСТИ ФОРМИРОВАНИЯ МИКРОСТРУКТУРЫ ГРАНУЛИРОВАННЫХ ЗАПОЛНИТЕЛЕЙ НА РАЗНЫХ ВЯЖУЩИХ КОМПОЗИЦИЯХ (ЧАСТЬ 3) В результате теоретического анализа установлено, что плотное зарастание кристаллической массой пор гранулированных заполнителей осуществляется при добавлении ВК-3 в количестве 15 % не зависимо от фракционного состава кварцевого песка. Микроструктура контактного слоя ГЗ с шифром 0,16+15 % ВК-3

Results
Conclusion
Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call