The article presents the results of studies on the structuring process of triple co-oligomers of styrene, isoprene and glycidyl ether of 4-isopropnylphenol, diethylenetriamine. The effect of temperature, amount of iethylenetriamine,and time of structuring of co-oligomers and the formation of copolymers with a cross-linked three-dimensional structure has been studied. It has been established that cross-linked copolymers can be synthesized with a yield of up to 90-97% by carrying out the process of structuring co-oligomers with iethylenetriamine at a temperature of 80-100°C for 3-5 hours.