Abstract
The study results of grinding the surfaces of gas turbine engine repair parts made of heat-resistant stainless steel EP-517SH with sprayed high-strength wear-resistant VKNA and VK-20KS coatings are considered in order to select the most effective abrasive tools. The effectiveness was evaluated based on the results of comparative studies of the quality parameters of the surface layer: roughness, cracking, tempering, peeling of the coating, pore formation, as well as the machining temperature when using grinding wheels made of fused alumina impregnated with molybdenum disulfide and without impregnation, made of green silicon carbide and el'bor borazon material. As a result of the study, it is found that the best quality of machining parts coated with VKNA and VK-20KS is achieved by using el'bor borazon circles.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.