Plastic weathering in the natural environment is a dynamic and complex process, where the release of microplastics, nanoplastics and additives poses potential threats to ecosystems. Understanding the release of different weathering products from plastics is crucial for predicting and assessing the environmental hazards of plastics. This study systematically explored these phenomena by exposing polystyrene (PS) to UV irradiation and mechanical agitation for different durations (1 day, 5 days, 10 days, 20 days). The degree of aging, yellowing, brittleness, and the abundance of carbonyl (CO) functional groups in PS were all gradually increasing over time. The weathering pattern of PS surfaces manifested as initial particle oxidation followed by later cracks or flakes formation. The release of products was positively correlated with the aging degree of plastics, as well as among the various released products. Laser infrared and Raman tests indicated that, for microplastics, the size range of 10–20 μm consistently dominated over time, while the primary size range of nanoplastics shifted towards smaller sizes. Additives and other soluble products were prone to release from weathering plastics, with 20 different chemicals detected after 20 d. The release of plastic additives was closely related to aging time, additive type, and quantity. This study contributes to our understanding of the weathering process of plastics, clarifies the release patterns of products over time, and the relationships among different products. It helps predict and assess the environmental pollution caused by plastics.
Read full abstract