In this paper, the influence of paraffinic oil on the physical mechanical and thermal properties of three EPDM rubbers types Buna EP T.6465, Keltan 5260Q and Keltan 6160 D have been investigated. The results showed that the tensile strength and the elongation at break of Keltan 5260Q and Keltan 6160 D with 10 phr paraffinic oil represent the improvement of 57.8% to 57.6% and 71% to 81% respectively, compared to EPDM rubbers without paraffinic oil. The mean peel force of EPDM keltan 6260D with 10 phr paraffinic oil loaded is about 36% and 32.5% higher than that of keltan 5260Q and EP.T 6465 respectively. Beside that at the suitable paraffinic oil contents, the thermal resistance of Keltan 5260 Q and 6160D seems to be a little higher than that of without processing oil and these EPDM rubbers are suitable for application to high thermal resistance rubber products.