1. The difference in csr size for FS and CS pressings is much less than that for the starting powders. The structural dissimilarity is apparently mainly due to a difference in the degree of development of grain and block boundaries. 2. The structural condition of CS and FS pressings causes differences in the propagation kinetics of primary and collective recrystallization in silver. The size of csr in sintered CS and FS pressings is approximately the same.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.