Abstract

This paper reports a new strainless fabrication method for ytterbium‐doped CaF2 laser ceramics involving no drying step before green body casting. The nanoparticles were kept in aqueous solution until green body shaping. Centrifugation was used to obtain correct compactness of the green body before sintering. Characterizations were conducted at different steps of the fabrication process. No grain boundaries oxidation was observed in the sintered ceramics although the nanoparticles were permanently maintained in water until they were sintered. Finally, these ceramics are more homogeneous and have less light scattering defects (no porosity), and present improved optical properties when compared to ceramics obtained from dried nanopowders.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.