Abstract

Zirconium oxide samples were sintered at two different temperatures (1250°C and 1450°C) using SPS method with maximum holding time 10 min. to obtain nonstoichiometric composition. Some of the samples were subsequently annealed for 6 hours at 1100°C to obtain stoichiometric composition. Wear rate and friction coefficient were obtained from tribological tests carried out on the UMT3 equipment (Bruker) using two different static partners (zirconia and alumina ball). Main aim of this work is to study the influence of composition and sintering temperature on the wear behavior, friction coefficient and basic mechanical properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.