Abstract

High quality and behavior of steel is playing an essential role in metal and manufacturing industries. Hardox steel has exceptional properties includes high wear resistant and hardness. The wear behavior of hardox 400 steel was evaluated through pin on disc tribometer using different input constraints such as load, sliding velocity and disc speed. The wear worn surface was investigated through atomic force microscopy. The wear rate of the hardox steel was calculated with different load conditions. The wear factors and wear rate were optimized by taguchi method. Variance analysis was provided the contribution of each factor on mass loss.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.