The P2- and O3-Na0.67Co0.33Ti0.67O2 cathodes undergo a very slow transformation during charge and discharge in sodium batteries due to a valence and spin-state transition of cobalt cations. As a result, a big potential hysteresis of 2.5–3 V arises.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.