Abstract

This work aimed to study the UV-laser treatment of precursor (i.e. nanodiamond (ND) seeds on silicon substrates) and its influence on the properties of grown nanocrystalline diamond (NCD) films. Pulsed Nd : YAG laser operating at the fourth harmonic frequency (laser fluence EL = 250 mJ cm−2, pulse duration 5 ns) was used as a source, equipped with an optical system for focusing laser beam onto the sample, allowing exposure of a local spot and horizontal patterning. The variable parameters were: number of pulses (from 5 to 400) and the working atmosphere (He, Ar and O2). Ablation and/or graphitization of seeded nanodiamond particles were observed. Further the microwave plasma-enhanced chemical vapour deposition was employed to grow NCD films on exposed and non-exposed areas of silicon substrates. The size, shape and density distribution of laser-treated nanodiamond seeds were observed by atomic force microscopy (AFM) and their chemical composition by x-ray photoelectron spectroscopy (XPS) analysis. The resulting NCD films (uniform thickness of 400 nm) were characterized by: Raman spectroscopy to analyse occurrence of graphitic phase, and AFM to observe morphology and surface roughness. The highest RMS roughness (∼85 nm) was achieved when treating the precursor in He atmosphere. Horizontal microstructures of diamond films were fabricated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.