[Title: TEST UV-VIS LAYER TiO2/N2 FOR DETERMINING BAND GAP ENERGY] The effect of nitrogen doping variation on energy band gap in TiO2 layer grown by doctor blade technique. The TiO2/N2 layer was prepared with concentrations of 0%, 15%, 25% and 25% calcined at 500°C for 3 hours. Characterization of band gap energy by using the UV-Vis spectrometer at a wavelength range of 200 nm-700 nm. The band gap energy is obtained by using the Swanepoel equation and Touch Plot method. The results showed that doping of nitrogen can decrease the band gap energy of 3.9250 eV, 3.8750 eV, 3.8375 eV and 3.9125 eV, respectively. The smallest energy band gap is obtained at 25% concentration that is 3.8375eV.
 Keywords: Coating TiO2/N2, transmittance, Band gap energy

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.