Abstract

AbstractFor high temperature thermoelectric applications, Yb14MnSb11 has a maximum thermoelectric figure of merit (zT) of ∼1.0 at 1273 K. Such a high zT is found despite a carrier concentration that is higher than typical thermoelectric materials. Here, we reduce the carrier concentration with the discovery of a continuous transition between metallic Yb14MnSb11 and semiconducting Yb14AlSb11. Yb14Mn1‐xAlxSb11 forms a solid solution where the free carrier concentration gradually changes as expected from the Zintl valence formalism. Throughout this transition the electronic properties are found to obey a rigid band model with a band gap of 0.5 eV and an effective mass of 3 me. As the carrier concentration decreases, an increase in the Seebeck coefficient is observed at the expense of an increased electrical resistivity. At the optimum carrier concentration, a maximum zT of 1.3 at 1223 K is obtained, which is more than twice that of the state‐of‐the‐art Si0.8Ge0.2 flown by NASA.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.