Abstract
This paper presents a concept for performing three-dimensional laser machining on composite materials, using two intersecting laser beams to create grooves on a workpiece. A volume of material is removed when the two grooves converge. An analysis of the grooving process was conducted for carbon/teflon and glass/polyester materials. A model was developed to determine groove depth from process parameters and material properties. Close agreement was found between model predictions and experimental results for groove depths in carbon/teflon. Model predictions consistently overestimated depth values for continuous-beam glass/polyester results, and underestimated depth values for pulsed-beam glass/polyester at low power/high speed. Corrections for heat losses and high-temperature chemical interactions were added to the model to improve agreement with data. Groove width and damage width results were compared with surface quality standards for laser cutting of composites.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.