Abstract

ABSTRACTThermoplastic vulcanizates (TPVs) based on high‐density polyethylene (HDPE), ethylene–propylene–diene terpolymer (EPDM), and ground tire rubber (GTR) were dynamically vulcanized with dicumyl peroxide (DCP). The polymer blend was composed of 40% HDPE, 30% EPDM, and 30% GTR, and the concentration of DCP was varied from 0.3 to 3.6 parts per hundred rubber (phr). The properties of the TPVs were determined by evaluation of the gel fraction content and the mechanical properties. In addition, IR spectroscopy and differential scanning calorimetry analysis were performed as a function of the DCP content. Decreases in the Young's modulus of the blends and the crystallinity of HDPE were observed when the content of DCP was greater than 1.8 phr. The results regarding the gel content indicate that the presence of DCP promoted the crosslinking of the thermoplastic matrix, and optimal properties were obtained with 1.5% DCP. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 39901.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.