A water-quenching technique was adopted to evaluate the thermal shock behavior of as-sintered and pre-oxidation Zr 2Al 4C 5–20 vol.%SiC composites in an air atmosphere. The strength retention of the two kinds of composites was measured after varying temperature (Δ Tc) up to 800 °C. As-sintered Zr 2Al 4C 5–20 vol.%SiC showed rapidly drop in flexural strength above Δ T of 400 °C. However, the pre-oxidation Zr 2Al 4C 5–20 vol.%SiC composite showed a higher retained strength up to 800 °C, and the critical thermal shock temperature difference (Δ Tc) is as high as 660 °C. The main reasons for a great improvement of thermal shock resistance (TSR) were also discussed and analyzed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.