Abstract

This paper reports the growth, thermal and polarized spectral properties of Cr3+:MgWO4 crystal. Cr3+:MgWO4 crystal with dimensions of 20×18×13mm3 was grown successfully by a top-seeded solution growth method. The average thermal expansion coefficients are 10.47×10−6K−1, 15.68×10−6K−1 and 10.75×10−6K−1 along a-, b- and c-axis, respectively. The thermal conductivity is 8.69W/(mK) at room temperature. Both of the absorption and emission spectra show strong polarization characteristics. There is a broad and strong absorption band at around 790nm, which means that Cr3+:MgWO4 crystal is suitable for AlGaAs laser diode pumping. The crystal has a broad emission band at 961nm with a full width at half-maximum of 202nm; the emission cross-section is about 1.8×10−19cm2. The results show that Cr3+:MgMoO4 crystal can be regarded as a potential tunable laser gain medium.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.