Abstract

SiO2 was extracted from kaolin using concentrated HCl and HNO3 mixture and used as solid support for both Bronsted (HClO4 and H2SO4) and Lewis Acid (AlCl3 and ZnCl2). Before extraction, kaolin was calcined at 800°C for eight hours to form metastable kaolin. After the extraction procedure, silica was recovered in 51.6% yield. Silica and the resulting solid acids were then characterized using XRD, XRF, and FTIR. XRD pattern shows that silica synthesized from kaolin is in the mixture of amorphous and α-quartz silica. Immobilization of acids alters its structure becomes more crystalline. XRF analysis shows that the loading of AlCl3 and ZnCl2 was 9.5 and 24.8%, respectively. The acid catalysts were then used in the esterification reaction of 4-hydroxybenzoic acid with sucrose. The reactions were conducted in dimethyl sulfoxide (DMSO) solvent by varying reaction time and reaction temperature. The highest conversion of starting materials and selectivity towards ester was obtained over the AlCl3/SiO2 catalyst. DPPH radical scavenging test shows that the ester exhibits good antioxidant activity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.