Abstract

Microchemistry and microstructure of TiN in Alloy 690TT were analyzed using SEM and TEM. Constant loading test was conducted on Alloy 690TT in 325 °C water to study effect of TiN on SCC initiation. It was found that TiN-inclusion stringers existed along the longitudinal axis. Numerous micron-size TiN with Al 2O 3 and/or MgO nuclei and submicron-size TiN existed in this alloy. After holding a constant load equal to 180% of the yield strength for 40 days, cracks about 1–3 μm initiated at micron-size TiN and TiN-inclusion stringers in the near surface. The mechanisms of Alloy 690TT crack initiation at these TiN are discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.