Abstract

The casting defects, microstructure and hardness of Elektron 21 Mg sand casting alloy was investigated. Visual and radiographic examination showed the presence of non-metallic inclusions and porosity. Quantitative analysis of microstructure was performed, no correlation between section thickness, grain size, volume fraction of eutectic areas and hardness was observed. Casting defects were responsible for cracking at magnesium casting/steel tube interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.