Abstract

In this experiment, ZnO thin films were sputtered on a glass substrate by a radio frequency (RF) magnetron sputtering system at room temperature (RT). The thicknesses (tf) of the ZnO thin film were from 500Å to 1000Å. X-ray diffraction (XRD), ultra miniature spectrometer (Spactra Smart) and four-point probe measurements were used to investigate the characteristics of ZnO thin film with various thicknesses. The results exhibited that ZnO has a wurtzite structure with a (002) texture diffraction peak in the 2θ at 34° range. As the ZnO thin film thickness increases, the grain size becomes larger. A ZnO thin film thickness of 500Å had a transmittance maximum of about 85% and a reflectance minimum of about 15%. That means that thickness and crystallinity of ZnO play an important role in the optical results. Additionally, the four-point probe measuring resistivity (ρ) found that the ρ is reduced as the ZnO thickness increases because grain boundaries and the surface of thin films scatter the electrons, so thinner films have a greater resistance. Between grain size and the nanoindentation results, the decline in the hardness and Young's modulus can be reasonably concluded to be associated with an enlarged grain size, consistent with the “Hall–Petch” effect and the grain refinement mechanism. Based on the optical, electrical, and nanomechanical results, a thickness of 500Å of ZnO is suitable for photoelectrical application.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.