Abstract
The galvanic corrosion behavior of titanium (TA2)/Cu-Ni alloy (B10)/low alloy steel (921A) multi-material system has been studied using a zero-resistance ammeter (ZRA) in seawater at different temperatures. After the tests, the surface morphologies of the samples were detected by SEM. Results showed galvanic corrosion behavior of TA2/B10/921A fulfill the mixed potential theory, 921A acts as the anode and both TA2 and B10 act as the cathodes. The effect of temperature on the galvanic corrosion is important, the corrosion rate increases with increasing temperature.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.