Materials and Methods: Based on ADA specification #27, 50 identical 25×2×2 mm samples were fabricated from five interim materials (TempSpan, Protemp 4, Unifast III, Trim and Revotek LC) and stored for 14 days at 37°C in three different mouthwashes (Listerine, Oral B and Chlorhexidine) and distilled water (control group). After conditioning, the flexural strength values were assessed by a universal testing machine. The standard three-point bending test was conducted on the specimens at a crosshead speed of 0.75 mm/min. Data were statically analyzed by the two-way ANOVA and Tukey HSD tests. Results: The mean ranks of flexural strength of the examined materials were as follows: TempSpan= 121.10, Protemp 4= 111.93, Unifast III= 63.44, Trim= 62.83 and Revotek LC= 46.55.There was no significant difference between Unifast III and Trim, however; the other materials showed significant differences. Both bis-acryl resin composite materials showed higher flexural strength than the methacrylate and light-cured resins after 14 days storage in mouthwashes. One of the bis-acryl resins (TempSpan) showed the highest flexural strength. The light polymerized resin (Revotek LC) presented the least flexural strength. Conclusions: The mouthwashes employed in this study did not show any statistically significant effect on the flexural strength of the five tested interim materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.