At the entrance temperature of 300°C, the effect of mill temperature on the texture and microstructure evolution was worked to 85/15 α-brass by two rollings with mill temperatures calibrated as 28°C for one rolling and 55°C for another, in which TEM was employed to reveal the microstructures, and ODF to represent the related textures. From the experiment evidence, a detailed discussion was made and led to a conclusion: in current rolling, with recovery, mill temperature influences the rolling texture and microstructure development through chilling and the working temperature induced deformation mechanisms change, the former one affecting B intensities, by contrast, the latter one leading to a texture transition.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.