ABSTRACT The results of a study of environmental ageing on the apparent interfacial shear strength of glass fibre–vinyl ester microbond samples are presented. The scale related issues of estimating water absorption levels in microbond samples are reviewed and discussed and a solution based on Fickian diffusion is given. Interphase strength of microdroplets aged in water at 23°C was relatively stable up to 6 days exposure after which strength degradation was fairly rapid. Immersion in water at 50°C resulted in an immediate 20–30% irreversible loss of strength. Further exposure beyond 2 days led to total loss of integrity of the microbond samples. Electron microscope images of aged microdroplets appeared to show the development of a bi-phasic microstructure. The presence of two phases in small scale vinyl ester polymer samples was confirmed by DMA on thin films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.