Abstract
The TiN thin film is considered a promising electrode layer for 3D capacitors. In this study, TiN thin films were prepared on Si substrates using atomic layer deposition (ALD) at various temperatures from 375 °C to 475 °C. The crystallization behavior, microstructure, and conductance properties of those TiN thin films were investigated. The resistivity of TiN thin films deposited on Si wafers can reach as low as 128 μΩ·cm. TiN thin films showed lower resistivity and worse uniformity with the deposition temperature increasing. In addition, the aging of TiN thin films may weaken the device performance. Optimized deposition parameters were found and full-coverage deposition of thin films on the wall of deep holes with an aspect ratio of approximately 14 has been successfully achieved. The results would be a good reference for the development of 3D capacitors and other microelectronics components.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.