The ceramic coating containing anatase TiO2 and rutile TiO2 is fabricated on the surface of pure titanium in the electrolyte of C4H6CaO4-NaH2PO4 by micro-arc oxidation (MAO) method. The effect of different current density to microscopic structure, elemental composition and phase components of Ceramic Coating are studied with scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), 3D profilometer and etc. Results indicate that the ceramic coating on pure titanium by micro-arc oxidation is a porous mixed crystal structure which is mainly composed of such elements as Ti, O, Ca and P. With current density increasing, the average pore diameter and roughness on film surface first increase and then decrease, the porosity increases, the ratio of Ca/P then decreases, the relative content of anatase TiO2 increases and that of rutile TiO2 decreases.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.