Abstract

The relative permittivity of O-cresol Novolac epoxy resin/(Ba0.9Sr0.1)(Ti0.9Zr0.1)O3 (epoxy/BSTZ) composites with various contents of BSTZ ceramic powder was measured at 10 kHz to 1 MHz. As the content of BSTZ ceramic powder increases from 0 to 70 wt%, the permittivity increases from 5.72 to 25.23. Four different mixing rules are used to predict the variation of permittivity of epoxy/BSTZ composites, and the Lichtenecker equation fits the measured results. The permittivity of epoxy/BSTZ composites slightly increases as the measured temperature increases, and is unchanged when the measured temperatures are higher than the Curie temperature of BSTZ ceramic. This research proves that we can develop the epoxy/BSTZ composites with characteristics of stable temperature and frequency dependence.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.